HS Code |
697058 |
| Product Name | Polyvinyl Alcohol Film GH-17Y |
| Appearance | Transparent film |
| Thickness | 17 microns |
| Width | Standard rolls, customizable |
| Density | 1.26 g/cm³ |
| Solubility | Cold and hot water soluble |
| Tensile Strength | Approx. 120 MPa |
| Elongation At Break | 60% |
| Moisture Content | 5-8% |
| Ph | 5-7 |
| Biodegradability | Biodegradable |
| Heat Sealability | Excellent |
| Residual Monomer Content | <0.1% |
As an accredited Polyvinyl Alcohol Film GH-17Y factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyvinyl Alcohol Film GH-17Y is packaged in sealed plastic bags, 100 sheets per box, labeled with product name and handling instructions. |
| Shipping | Polyvinyl Alcohol Film GH-17Y is typically shipped in sealed, moisture-proof packaging to prevent contamination and degradation. Rolls or sheets are securely boxed and cushioned to avoid damage during transit. Labels indicate product details and handling precautions. Shipments comply with safety and environmental regulations, ensuring safe delivery to industrial or laboratory destinations. |
| Storage | Polyvinyl Alcohol Film GH-17Y should be stored in a cool, dry, and well-ventilated area, away from direct sunlight and moisture. Keep the film in tightly sealed containers or original packaging to prevent contamination. Avoid exposure to strong oxidizing agents and excessive heat. Ideal storage temperatures range from 5°C to 35°C to maintain product quality and stability. |
| High Purity: Polyvinyl Alcohol Film GH-17Y with 99% purity is used in pharmaceutical packaging, where it ensures non-toxic and safe containment. Dissolution Rate: Polyvinyl Alcohol Film GH-17Y with rapid dissolution is used in detergent pod manufacturing, where it guarantees efficient and residue-free release of contents. Tensile Strength: Polyvinyl Alcohol Film GH-17Y with high tensile strength is used in food packaging, where it provides robust mechanical protection during transportation. Moisture Barrier: Polyvinyl Alcohol Film GH-17Y with low water vapor transmission rate is used in electronics packaging, where it protects sensitive components from humidity. Biodegradability: Polyvinyl Alcohol Film GH-17Y with certified biodegradability is used in single-use medical applications, where it enables environmentally responsible disposal. Thermal Stability: Polyvinyl Alcohol Film GH-17Y with stability at 150°C is used in lamination processes, where it maintains film integrity under heat treatment. Viscosity Grade: Polyvinyl Alcohol Film GH-17Y with a viscosity of 35 mPa·s is used in adhesive formulations, where it allows for uniform spreading and strong adhesion. Thickness Uniformity: Polyvinyl Alcohol Film GH-17Y with 0.03 mm consistent thickness is used in precision coating operations, where it delivers predictable dissolution rates. Molecular Weight: Polyvinyl Alcohol Film GH-17Y with 85,000 g/mol molecular weight is used in textile sizing, where it provides optimal fiber coating and wash-off performance. Transparency: Polyvinyl Alcohol Film GH-17Y with 92% light transmittance is used in optical-grade packaging, where it ensures clear product visibility. |
Competitive Polyvinyl Alcohol Film GH-17Y prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please call us at +8615371019725 or mail to admin@sinochem-nanjing.com.
We will respond to you as soon as possible.
Tel: +8615371019725
Email: admin@sinochem-nanjing.com
Flexible payment, competitive price, premium service - Inquire now!
Working on the production floor and in the lab, it's easy to spot small details that separate strong polyvinyl alcohol (PVA) films from those that just look similar on paper. Each batch teaches something new about the material, its reaction to heat, humidity, tension, and the demands of engineers and operators working downstream. That hands-on experience led us to develop and refine our Polyvinyl Alcohol Film GH-17Y, a film that matches real expectations from manufacturing lines in industries as diverse as agriculture, textiles, packaging, and cleaning products.
Many customers come to us after basic PVA products fail to meet everyday processing pressures. They bring mishaps: inconsistent solubility, uneven thickness, brittle sections, lack of control during winding or cutting, wrinkling during application, and sticky jams that rack up extra downtime. The difference with GH-17Y can be traced to gradual adjustments made during manufacturing—small tweaks in polymerization temperature, precise water content controls, closely tracked stretch ratios, and recipe shifts based on feedstock behavior from month to month. Every drum and bag of raw material becomes part of a continuous feedback loop. What matters most to users is the end film’s consistency and reliability in practice, not just in a lab test.
At our plant, quality is checked not only by lab technicians but directly in the factory bays. We learned that operators prize a film that reels off without static, carries a predictable fold pattern, and responds well to ultrasonic or heat sealing. GH-17Y was born out of that factory-floor dialogue. It pours easily onto winding rollers, never clings to cutting blades, and moves from storage into production with very little climate adjustment. Resistance against tearing during transport and handling is key, since real usage often involves trucks, containers, and hands wearing thick gloves.
Engineers in detergent pod factories highlighted a simple trouble: Some films dissolve with too much foam, or break open inside packaging. GH-17Y holds tight to formulations, delivering burst release only when needed—after full immersion, not during storage or at slight humidity upticks. The backbone of this is in the film’s evenness and pore structure, which results from process controls at every phase: everything from the resin blend and casting head temperature, right through to slow, carefully managed drying in long ovens. We check solubility not just with lab water but with all kinds of tap and softened water samples, to make sure the film reacts correctly outside controlled settings.
Clients rarely walk in asking about molecular weights or degrees of hydrolysis—they come in with problems from their machines or complaints from their own clients. That’s where the GH-17Y grade stands out. Its thickness range fits standard filling lines and forms pocket shapes reliably. We keep tight tolerance on thickness because it affects solubility and mechanical strength—hard-won knowledge after seeing the damage a tenth of a millimeter off-target can cause.
GH-17Y absorbs shock and stress during bag and pod forming, thanks to a stretch profile refined over hundreds of test runs. Color stability is also critical for visual inspection; our board pays close attention to eliminating streaks or discoloration. Food packaging trials reminded us how sensitive end customers are to odors, so we eliminated unwanted volatile compounds through careful selection of plasticizers and washing steps during slurry preparation. After examining failures from dozens of different regions, we built up resistance in GH-17Y to real-world storage and shipping—deep freezes, hot and damp containers, even long haul transits through climate extremes.
Many competitors operate under the illusion that PVA films are interchangeable, so they purchase material from generic batches with only broad controls. Our team knows every extruder, reactor, and finishing machine in the plant, and every product grade has evolved in answer to years of specific customer feedback. We spent six months testing new casting blocks to smooth out flow lines that sometimes caused breakage in earlier versions of PVA film. It wasn’t enough to pass a few tensile strength checks; we wanted GH-17Y to withstand the vibration and jostle that comes with industrial packaging and bulk handling.
Every operator on our floor understands they’re accountable for detecting pinhole defects or surface roughness. We sponsor in-house workshops focusing on practical skills, like recognizing minor color shifts caused by resin lot changes or spotting early signs of edge curling. That’s how the quality story of GH-17Y differs from film put together as a rushed afterthought.
What really sets PVA film GH-17Y apart is its targeted dissolution profile. Industry partners in water-soluble detergent packaging, seed tape coiling, and even electronics cleaning have unique needs for timed release. The GH-17Y blend dissolves cleanly in both cold and warm water, but doesn’t turn sticky in moist air. This demands precision at the macromolecular level, as we balance mechanical durability with quick and clean breakdown when submerged.
We worked with researchers and downstream users to test GH-17Y with a wide variety of fillers, dyes, and active ingredients. The film stands up to mild acids and bases, retaining stability until it meets its designed breaking point. Every trial batch passes tests that go beyond ISO or industry standard: on-site customer simulation runs, and temperature cycling that pushes the film through weeks of simulated warehousing and shipping. Many standard-issue films fail here – GH-17Y stays true to its original dissolution profile, batch after batch.
The move to GH-17Y often stems from the desire to reduce microplastic residue, improve end-of-life solutions, and create safer user environments in facilities and homes. That’s not marketing fluff: We built the film formula with water solubility as a guiding principle, using additives proven for minimal residuals. GH-17Y breaks down without leaving visible shreds, powder, or cloud—an important assurance for agricultural seeding and medical laundry applications, where film remains in soil or in critical water systems.
Customers in high-volume packaging processes also face dust, static, and film cuttings that can collect on surfaces or inside machinery. The GH-17Y recipe tackles static cling, reduces debris, and handles offcuts neatly. It doesn’t just leave equipment cleaner. The difference is seen in reduced line stoppages, less maintenance, and a lower chance of defective final products caused by contamination from old film residue or fibrous breakdown.
The strength of Polyvinyl Alcohol Film GH-17Y impacts everyday handling. The actual pull tests—by hand, not just on lab equipment—help us understand how the film stretches and resists tears when loaded onto automated forming machines and during manual pouch stuffing. The film’s modulated plasticizer system fixes common problems such as brittleness and uncontrolled snap-back. Users have noted significantly fewer broken pouches since switching, especially on older lines that run hotter seal temperatures or have erratic pressure bars.
We observed over time that film with less predictable shrink or curl wastes more operator time, causes interruptions during high-speed production, and fouls up downstream filling. GH-17Y’s shrinkage stays in line with processing requirements. Operators don’t waste extra minutes realigning film every batch or fiddling with climate controls. This helps maintain throughput, keeps waste rates low, and lets smaller teams manage the entire forming and packing cycle.
Each cycle of GH-17Y’s production brings a new opportunity to improve resource use. We actively recapture scrap, recycle wash water, and limit solvent discharge at every stage. Our process designs grew out of real audits by waste disposal teams and environmental compliance officers who spotted bottlenecks and material loss points early. The film uses only safe, registered additives, and adheres to tested migration limits suitable for use with detergents, seeds, and some food contact packaging.
Customers worldwide have asked us about the end fate of water-soluble film, especially for agricultural or specialty cleaning products. GH-17Y decomposes fully in working wastewater conditions, right down to small molecular building blocks that don’t accumulate or linger on equipment or land. We track feedback from downstream users and regulators in multiple countries to continually verify that the film meets not just written law but also the rising needs and public concern about microplastics and persistence.
Facilities running short shift rotations or managing multiple film feedstocks can’t always afford single-purpose equipment. Here, GH-17Y makes a difference by feeding cleanly through both older and modern lines. We worked with operating teams to identify common tweaks that could be made mid-run without excess stoppage. Our lab teams routinely mix GH-17Y with common inks, dyes, and heat seal adhesives, ensuring that print clarity and edge definition hold up through storage and handling. This responsive approach removes much of the tension between film production and the changing needs of different sectors.
In specialty production, unpredictable switchovers can be a huge pain point. GH-17Y handles quick transitions and resists cross-contamination from other commonly processed films. Its lack of oily residue lets downstream pumps, applicators, and printers stay cleaner, reducing downtime when one product moves to another. As a result, operations teams gain flexibility without having to constantly overhaul their calibration or cleaning regimes.
Years of direct work with customers taught our engineers to look beyond generic product metrics. We know that downtime and end-of-line rejects mean real money and missed deadlines. That’s why GH-17Y is backed by a line-up of hands-on specialists who answer calls from operators, not just purchasing staff. As soon as a batch leaves quality control, we keep tabs on customer feedback—problems with roll handling, machine stoppages, or unexpected failure patterns. Customers value the direct support that only comes from a manufacturer willing to visit production lines and look at loading, infeed, and tensioning first-hand.
We take failures seriously. After a few unfortunate incidents with broken end seals in a large laundry capsule factory, we launched a task team to overhaul drying protocols and consult on real-world sealing parameters. Through that conversation, GH-17Y came back stronger, and it gave us insight into developing guidance for dealing with fluctuating local water qualities—something never visible in standard lab conditions.
Basic PVA films, especially those sourced from bare minimum suppliers, often fall short during prolonged exposure to humidity, hot storage, or active chemicals. With GH-17Y, we made sure that the material doesn’t stick, compress, or clump even after long periods on warehouse racks. Users in the seed tape sector, for instance, noticed fewer jams and more regular laydown patterns after switching, saving entire shifts that previously spent time detangling failed runs.
With detergent pods, improvements went beyond just the first-fill test. Our film protected active ingredients from air and light, holding performance over months of shelf-life studies. Sheets stayed flat and free from curl, so pods form round and symmetrical each time. That attention to subtle, accumulative issues means more operational peace of mind for bulk packers—no costly recall runs, less need for sorting, and less waste out the door.
The GH-17Y didn’t appear out of a single laboratory breakthrough. We built it through repeated trials, mistakes, and active conversations with everyone from factory operators to logistics managers. Piecing together the final formula required hundreds of tracked production cycles, factoring in seasonality, shifts in materials, and integrating feedback from the broadest range of industry users we could find. Each iteration of the film involved tweaks at the chemical, mechanical, and finishing stages, with quick pivots if test lots didn’t meet expectations under real conditions.
True progress relies on active trouble-shooting. We gather ongoing statistics on film performance: shrinkages by batch, complaint trends by region, time-between-failure on fill lines, plus methods for measuring how quickly and cleanly pouches dissolve in final-use environments. This level of control—bolstered by transparency and quick adaptation—reduces the gap between what users need and what standard films actually deliver.
As markets and regulations evolve, the demand for water-soluble and biodegradable films continues to grow. With GH-17Y, we stand firmly behind a product that fits into sustainable production cycles while meeting the tight performance requirements of modern packaging, agriculture, and specialty cleaning. Feedback from our clients shapes our next improvements. This feedback-driven cycle means GH-17Y will keep moving forward to meet not only today’s challenges, but tomorrow’s as well.
Whether you are running a high-throughput packaging line, managing fleets of washing capsules, or looking for new ways to integrate dissolvable film into specialty products, the lessons learned from producing GH-17Y have always pointed to one truth: Talk directly with operators, listen to daily pain points, and stay ready to make changes fast. It’s real results—not just technical promises—that drive each batch out the door.